Cold Shut
What it is:
A surface defect of a metal casting in the form of a discontinuity where two streams failed to unite.
Causes:
Improper cleaning in the cast and/or a cast at the end of its lifecycle.
Solutions:
Chem-Trend’s solutions can help alleviate Cold Shut issues as well as extend the life of your metal casting equipment.
RELATED CASE STUDIES
Chem‑Trend develops, produces and distributes complex, explanation-intensive chemical products and addresses exclusively commercial customers (B2B). This website is intended solely for information purposes for professionally experienced readers in a B2B context and is not intended for consumers. The information contained herein is based on Chem‑Trend’s general experience and knowledge at the time of publication and does not constitute binding specifications, guarantees or warranties. Website information and documents contained herein are confidential and shall not be disclosed, reproduced or forwarded to any third party without the prior explicit written approval of Chem‑Trend.
© 2026 Chem‑Trend L.P. or Chem‑Trend affiliated company. All rights reserved.
Regional websites:
-
Argentina
-
Brasil
(Brazil) -
Canada
-
Česko
(Czech Republic) -
CIS (excluding Russia)
-
Deutschland
(Germany) -
España
(Spain) -
France
-
India
-
Italia
(Italy) -
México
-
România
(Romania) -
Polska
(Poland) -
Türkiye
(Turkey) -
United Kingdom
-
United States
-
Việt Nam
(Vietnam) -
中国
(China) -
한국
(South Korea) -
日本
(Japan)
Notice
You are about to exit this page. You will be redirected to the Chem‑Trend Global website where you’ll find your requested content in English.
Continue